PROPERTY HGS TYPE SPECIFIED VALUES AS PER IS:2046 - 1995 CRAFTWOOD CONFIRMS
PROPERTIES 1 MM (+/-10%) ✓
Resistance to surface wear 350 (revolution) ✓
Resistance to immersion in boiling water
- Mass increase (%)
- Thickness Increase (%)

10.0 Max
11.8 Max
✓
Resistance to dry heat 180 degree C Not a worse than 4 ✓
Dimensional stability at deviated temperature
- Longitudinal (%)
- Transverse (%)

0.5 Max
0.9 Max
✓
Dimensional Stability at 20 degree C
- Longitudinal (%)
- Transverse (%)

0.375 Max
0.60 Max
✓
Resistance to impact by small diameter ball 20 N Min ✓
Resistance to Cracking Not Worse than 4 ✓
Resistance to Scratching 2 N Min ✓
Resistance to staining Not Worse than 5 ✓
Resistance to color change (Wool standard)
- In Xenon arc light
- In enclosed carbon arc light

Not Worse than 6
Not Worse than 5
✓
Resistance to cigarette burns Not worse than 3 ✓
Resistance to steam Not worse than 4 ✓
Appearance Should be free from foreign particles ✓
PROPERTY HGS TYPE SPECIFIED VALUES AS PER IS:2046 - 1995 CRAFTWOOD CONFIRMS
PROPERTIES 1 MM (+/-10%) ✓
Resistance to surface wear 350 (revolution) ✓
Resistance to immersion in boiling water
- Mass increase (%)
- Thickness Increase (%)

10.0 Max
11.8 Max
✓
Resistance to dry heat 180 degree C Not a worse than 4 ✓
Dimensional stability at deviated temperature
- Longitudinal (%)
- Transverse (%)

0.5 Max
0.9 Max
✓
Dimensional Stability at 20 degree C
- Longitudinal (%)
- Transverse (%)

0.375 Max
0.60 Max
✓
Resistance to impact by small diameter ball 20 N Min ✓
Resistance to Cracking Not Worse than 4 ✓
Resistance to Scratching 2 N Min ✓
Resistance to staining Not Worse than 5 ✓
Resistance to color change (Wool standard)
- In Xenon arc light
- In enclosed carbon arc light

Not Worse than 6
Not Worse than 5
✓
Resistance to cigarette burns Not worse than 3 ✓
Resistance to steam Not worse than 4 ✓